Engineering - Material Properties

Bearing, gear & cutter life extended by 200 - 500%.


Composition - Modified Tungsten Disulphide (WS2 ) in laminar form.

Coefficient of Friction - 0.030 dynamic, 0.070 static. ( WS2 on WS2 )

Load Capacity - Same as substrate up to 350,000 psi

Adhesion - Molecular bond, no cure time, applied at ambient temperature

Temperature Range - Lubricates from -460oF to 1200oF ( -273oC to 650oC) in normal atmosphere, -350oF to 2400oF (-188oC to 1316oC) at 10-14 Torr

Chemical Stability - Inert, non-toxic, corrosion resistance. Non magnetic

Substrates - All ferrous and non ferrous metals, man-made solids /plastics

As A Substrate - Accepts most paints, all platings, is compatible with solvents, fuels and oils

LOX Compatibility - Insensitive to detonation by or in presence of oxygen

Hardness - approximately 30 Rockwell C

Thickness - 0.5 microns (0.000020 in)

Military Specification - Processed to DOD - L - 85645